Paint Finish Problems - Chalking (Whitening)
1. Chalking (Whitening)

Moisture in the air is concentrated in the paint film making the surface whitish, dulling the desired gloss.


CAUSES:
Using fast evaporating paint reducer/thinner during high temperature and humidity ambient conditions.
Spray gun air pressure too high.
Extremely cold paint surface.

PREVENTION:
Use high quality reducer/thinner with the correct evaporation rate (addition of an evaporation retarder can also help).
Properly set the spray gun’s air pressure.

CORRECTIVE ACTIONS:
If the symptom is not severe, add the retarder to the diluted paint and repaint. Or polish the paint surface with compound.
If the symptom is severe, sand down the paint surface after drying it thoroughly. Then repaint.